| dc.description.abstract | Fast urbanization in India poses a two-fold challenge: one is that there is an increase in the number of sites having poor quality soils, and the other is that the quantity of construction and demolition (C&D) waste resulting from such constructions has been rising steadily. Such problems need to be solved using advanced engineering practices. In this regard, the current research attempts to solve such a problem by investigating the use of crushed C&D waste as a stabilizer of a weak clayey soil obtained from Muzaffarpur, Bihar. Laboratory experiments were conducted on virgin clayey soil blended with C&D waste in varying proportions ranging from 0% to 28% (by dry weight). Comprehensive geotechnical tests were performed, including Atterberg's limit tests, Standard Proctor compaction tests, unconfined compressive strength (UCS) tests after 28 days of curing, direct shear tests, and falling head permeability tests, all in accordance with applicable Bureau of Indian Standards (BIS) codes. The findings reveal a consistent and progressive reduction in liquid limit (from 52% to 38%) and plasticity index (from 24% to 5%) with increasing C&D waste content, indicating improved consistency and reduced swelling potential. Compaction test results show a gradual decrease in both optimum moisture content and maximum dry density, attributed to the lower specific surface area and granular character of demolition waste. Most significantly, unconfined compressive strength improved substantially with C&D waste addition, reaching a peak value of 1352.68 kPa at 24% C&D Waste content — representing nearly a threefold increase over the untreated soil. This strength gain is primarily attributed to enhanced mechanical interlocking between soil particles and coarser C&D Wate fragments, supplemented by pozzolanic reactions V involving calcium-silicate compounds present in demolition debris. Permeability characteristics also improved, indicating better drainage potential in stabilized mixes. The study conclusively demonstrates that construction and demolition waste is a technically effective, economically viable, and environmentally sustainable alternative to conventional chemical stabilizers for improving the engineering behavior of clayey soils. Practical implementation of this approach can simultaneously address two pressing concerns: the treatment of weak foundation soils and responsible management of C&D waste through beneficial reuse. | en_US |
| dc.language.iso | en | en_US |
| dc.relation.ispartofseries | TD-9348; | - |
| dc.subject | SOIL STABILIZATION | en_US |
| dc.subject | CONSTRUCTION | en_US |
| dc.subject | DEMOLITION WASTE | en_US |
| dc.title | SOIL STABILIZATION USING CONSTRUCTION AND DEMOLITION WASTE | en_US |
| dc.type | Thesis | en_US |
| Appears in Collections: | M.E./M.Tech. Civil Engineering | |
Files in This Item:
| File | Description | Size | Format | |
|---|---|---|---|---|
| Vikram Anand M.Tech.pdf | 1.49 MB | Adobe PDF | View/Open | |
| Vikram Anand plag.pdf | 7.3 MB | Adobe PDF | View/Open |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.