Please use this identifier to cite or link to this item: http://dspace.dtu.ac.in:8080/jspui/handle/repository/23508
Full metadata record
DC FieldValueLanguage
dc.contributor.authorKUMAR, RAKESH-
dc.contributor.authorGautam, Vijay (SUPERVISOR)-
dc.date.accessioned2026-11-25T07:57:30Z-
dc.date.available2026-11-25T07:57:30Z-
dc.date.issued2026-09-
dc.identifier.urihttp://dspace.dtu.ac.in:8080/jspui/handle/repository/23508-
dc.description.abstractThis study offers a methodical examination of the mechanical properties, microstructural changes, and heated formability of laser-welded AA6082 Aluminium alloy tailor welded blanks (TWBs). Commercially obtainable sheets with thicknesses of 1.5, 2.0, 2.5, and 3.0 mm were utilized to create tailored welded blanks (TWB) including various thickness combinations (1.5×2.0 mm, 1.5×2.5 mm, and 1.5×3.0 mm) employing an industrial robotic fiber laser welding apparatus. Initial annealing trials determined 350°C to be the optimal pre welding thermal treatment, achieving an excellent equilibrium between strength (94 MPa yield strength) and ductility (19.8% elongation). Subsequent tensile analysis at high temperatures indicated that 300°C is the optimal temperature for warm forming. At this temperature, the substance demonstrated its peak elongation (28.2%) and a significant rise in the strain hardening exponent (n = 0.18), which is essential for facilitating uniform strain distribution and postponing localized necking. The refinement of laser welding parameters (3700-4000 W) resulted in flawless joints. Tensile tests validated exceptional weld integrity, with failure consistently manifesting in the thinner (1.5 mm) base sheet instead of the fusion zone. Microhardness assessments revealed concentrated hardening in the fusion zone (72-73 HV0.5) in contrast to the base metals (47-54 HV0.5), thereby effectively relocating the "weakest link" to the parent material. The assessment of stretch formability was conducted by Limit Dome Height (LDH) and Forming Limit Diagrams (FLD) at ambient temperature and under warm forming scenarios. Findings revealed that weld bead orientation is a more influential variable than temperature by itself; longitudinal weld alignment markedly enhanced LDH at 300°C, specifically by 49.6% for the 1.5 × 3.0 mm configuration, whereas transverse alignment exhibited minimal enhancement. The combinations examined, the 1.5 × 3.0 mm TWB exhibited the superior forming capability, attaining the maximum LDH (17.5 mm) and the most advantageous FLD at 300°C. Microstructural analysis by Electron Backscatter Diffraction (EBSD) demonstrated grain vi enlargement in the fusion zone (29.25 μm) relative to the base metals and heat affected zones (HAZs). Notwithstanding the bigger grains, the fusion zone retained its strength owing to a modest density of Geometrically Necessary Dislocations (GND) and its crystallographic texture. Ultimately, finite element analyses utilizing Abaqus/Explicit effectively forecasted strain distributions and failure sites, validating that warm forming at 300°C yields a more uniform strain distribution. This research indicates that the 1.5 × 3.0 mm longitudinal TWB created at 300°C yields the best balance of welding quality, mechanical properties, and warm forming characteristics.en_US
dc.language.isoenen_US
dc.relation.ispartofseriesTD-9302;-
dc.subjectAA6082 ALUMINIUM ALLOYen_US
dc.subjectTAILOR WELDED BLANKSen_US
dc.subjectELECTRON BACKSCATTER DIFFRACTIONen_US
dc.subjectLIMITING DOME HEIGHTen_US
dc.subjectFINITE ELEMENT ANALYSISen_US
dc.subjectFORMING LIMIT DIAGRAMen_US
dc.subjectLASER WELDINGen_US
dc.subjectWARM FORMINGen_US
dc.subjectANNEALINGen_US
dc.titleINVESTIGATIONS ON FORMABILITY OF TAILOR WELDED BLANKS OF ALUMINIUM ALLOY IN WARM WORKINGen_US
dc.typeThesisen_US
Appears in Collections:Ph.D. Mechanical Engineering

Files in This Item:
File Description SizeFormat 
Rakesh Kumar Ph.D..pdf6.26 MBAdobe PDFView/Open
RAKESH kUMAR PLAG.pdf6.52 MBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.