Please use this identifier to cite or link to this item:
http://dspace.dtu.ac.in:8080/jspui/handle/repository/23504Full metadata record
| DC Field | Value | Language |
|---|---|---|
| dc.contributor.author | GAUR, SHAILENDRA KUMAR | - |
| dc.contributor.author | MURTAZA, QASIM (SUPERVISOR) | - |
| dc.contributor.author | MISHRA, R.S. (CO-SUPERVISOR) | - |
| dc.date.accessioned | 2026-11-25T07:56:55Z | - |
| dc.date.available | 2026-11-25T07:56:55Z | - |
| dc.date.issued | 2026-06 | - |
| dc.identifier.uri | http://dspace.dtu.ac.in:8080/jspui/handle/repository/23504 | - |
| dc.description.abstract | In this thesis the investigation of structural, morphological, and nano-mechanical properties of vacuum evaporated cadmium telluride (CdTe) and Zinc Sulfide (ZnS) stack layers has been done. The films used for the fabrication of optoelectronic sensors in the infrared range. The films had been deposited by vacuum evaporation technique on Si (100) substrate. The X-ray diffractogram had indicated stable polycrystalline cubic structure with (111) preferential orientation for both films. The crystallite size, intrinsic stress, microstrain, and dislocation density values had been evaluated to be 17.5 nm, 0.09 GPa, 9.96, and 3.2 × 1011 lines/cm2, respectively, for CdTe film. While for ZnS film, the parameters had been estimated to be 15 nm, 0.49 GPa, 9.71, and 4.4 × 1011 lines/cm2, respectively. The Field Emission Scanning Electron Microscopy (FESEM) study had revealed homogeneous, dense, and defect free structure of the film. Compositional analysis had confirmed that the Te/Cd ratio 1.1 while S/Zn ratio 0.71 in the evaporated films. Atomic Force Microscopy (AFM) measurements had indicated smooth and uniform film with rms surface roughness of ~0.96 nm. Hardness, Young’s modulus, strain rate, and creep of the top layer (ZnS) had been evaluated by nanoindentation. The hardness of the ZnS film had evaluated to be 1.80 2.39 GPa, and Young’s modulus evaluated to be 181–248 GPa, for a 50–100 μN load. The outcome of the investigations endorsed the fact that the CdTe and ZnS thin films grown by the vacuum evaporation technique are suitable for the fabrication of optoelectronic devices. In second study, vacuum-sublimated cadmium telluride (CdTe) and zinc sulfide (ZnS) thin films were investigated at 1,5, and 10 Å/s evaporation rates to assess their suitability for mid- to long wave infrared device applications. X-ray diffraction analysis confirmed the formation of single phase, polycrystalline films with a face-centered cubic structure and a pronounced preferential orientation along the (111) crystallographic plane. Quantitative diffraction analysis revealed crystallite sizes of 21.4–19.4 nm for CdTe, with dislocation densities of 2.16 × 1011–2.63 × 1011 lines cm-2, residual stresses of 0.05– 0.19 GPa, microstrain values of 8.18–9.04, and stacking-fault probabilities of 3.80×10-3–4.19 × 10-3. The corresponding ZnS films exhibited crystallite sizes of 19.4–21.4 nm, dislocation densities of 3.18 × 1011–12.85 × 1011 lines cm-2, residual stresses of 0.20–0.44 GPa, microstrain values of 8.29–16.58, and stacking-fault probabilities of 4.23 × 10-3 8.48 × 10-3. Scanning electron microscopy revealed continuous and compact surface morphologies with high surface coverage and no discernible pinholes, particularly for films deposited under low temperature sublimation conditions. Energy-dispersive spectroscopic analysis further confirmed near-stoichiometric elemental compositions. Atomic force microscopy measurements showed root-mean-square surface roughness values of 0.84–7.40 nm for CdTe and 0.49–1.27 nm for ZnS. Optical transmission measurements demonstrated appreciable transparency over the 500–4000 nm spectral range, indicating their potential for infrared optical applications. The ex-situ residual stress measured using a multi-beam optical stress sensor (MOSS) was found to be 0.99–1.09 GPa for CdTe and 0.02–1.01 GPa for ZnS films. Nanoindentation measurements yielded hardness values 7 viii of 479–753 MPa and Young’s moduli of 63–141 GPa for CdTe, whereas ZnS exhibited hardness values of 150–478 MPa and Young’s moduli of 60–265 GPa. Furthermore, the creep response and strain-rate behavior of both films were evaluated to assess their mechanical stability. Electrical characterization of metal–insulator–metal (MIM) structures revealed a reduction in background leakage current from 1.5 × 10-6 A at ambient conditions to 1.8 × 10-7 A under liquid-nitrogen cooling, accompanied by an increase in relative permittivity from 6.90 to 7.94. At 77 K, the fabricated component structures exhibited leakage currents of 2.01 × 10-5 and 1.84 × 10-5 A, with stable capacitance values of 38–45 and 30–32 pF, respectively. Collectively, these structural, morphological, optical, mechanical, and electrical characteristics demonstrate the potential of vacuum-sublimated CdTe and ZnS thin films for development of infrared photonic and optoelectronic devices. In third experimental investigation, CdS nanoscale thin films were deposited on glass substrates at 1, 5 and 10 Å/s deposition rates by thermal evaporation process. XRD diffractogram indicate that the deposited CdS thin films have hexagonal structure with preferred orientation towards (002) plane and nearly stoichiometric composition. From XRD results, the calculated crystal structure parameters such as the crystallite size, microstrain and defect density were in the range of 20.4 14.7 nm, 7.74-10.62 and 2.3-4.52 × 1011 lines/cm2, at 1, 5 and 10 Å/s deposition rates, respectively. The AFM images indicated that the film’s rms surface roughnesses were 2.73 nm, 2.94 nm and 3.18 nm at 1, 5 and 10 Å/s, respectively. The SEM images indicated that the films were uniform, continuous and defect free. The EDX examination revealed that at 1 Å/s deposition rate the film was nearly stoichiometic. The optical band gaps were determined to be in the range of 2.37-2.43 eV. Nanoindentation tests evaluated the hardness, Young’s modulus, creep behavior and strain rate of CdS films. Hardness evaluated to be 0.14-1.48 GPa, 0.15-2.46 GPa, and 0.21-2.55 GPa at 1,5 and 10 Å/s deposition rate, respectively for 20-50 µN load. The Young’s modulus decreases 1-5 Å/s deposition rate and becomes almost constant 5-10 Å/s deposition rate at 70 µN loads. The characterization of CdS thin film recommends it as a favorable window layer in applications like photovoltaic, optoelectronic, thermoelectric and solar cells. As the requirement for high-performance, low weight, and efficient Infrared devices continues to rise, the formation of good ohmic is a critical step in fabrication of IR detector arrays. Structural and adhesion properties of tin (Sn) and indium (In) films and their contact formation on the n HgCdTe substrate are studied using the thermal evaporation technique in the fourth investigation work. The x-ray diffractogram indicated polycrystalline bcc phases with (200) orientation plane and (101) of β-Sn and indium films, respectively. The microstrain and dislocation densities were 4.10 and 9.10 x 1010 lines/cm2 and 3.83 and 9.03 x 1010 lines/cm2 of Sn and In, respectively. SEM examination indicated lumpy deposition of particle sizes from a few nanometers to microns in Sn film and uniform continuous films over the entire HgCdTe substrate with very small numbers of randomly oriented particles of 1-2 µm sizes in In film. EDS compositional analysis confirmed the presence of pure Sn and In films, respectively. Using AFM force microscopy in contact mode, adhesion force and thermodynamic adhesion work were 26.95 nN, 0.42 J/m2(DMT), and 0.57 8 ix J/m2(JKR) and 50.73 nN, 0.80 J/m2(DMT), and 1.07 J/m2 of In and Sn, respectively. Based on the transfer length method (TLM), the Sn/n-HgCdTe interface showed a higher specific contact resistance (ρc =2 x 10-2 Ωcm2) with nearly ohmic behavior, but the In/n-HgCdTe specific contact resistance of ρc = 3 x 10-4 Ωcm2 indicated that the In/n-HgCdTe interface exhibited ohmic features. Based on the experimental results, it was concluded that indium was the most suitable material to use for forming the ohmic n-contact in HgCdTe-based infrared detectors. In fifth study, the HgCdTe surface had been grown with small layers of gold using thermal evaporation and an e-beam process. The thermal and e-beam evaporated gold film exhibits a cubic face-centered cubic (fcc) structure along the (111) orientation, possesses favorable The thermally evaporated Au film's crystalline structural parameters such as defect density, residual stress, and microstrain were 1.8 x 1015-2.04 ×1015 lines/cm2, 0.24–0.26 GPa, 4.74–4.99, respectively while e beam Au film's defect density, residual stress, and microstrain were 1.27 x 1011-1.79 x 1011 lines/cm2, 0.02–0.31 GPa, and 3.94–4.67, respectively. The e-beam evaporated Au film had been the purest thin film with atomic 97.2 %. The e-beam gold film's uniformity, density, and extremely low roughness are confirmed by the AFM. The e-beam gold film's film-forming particles reached the appropriate lower grain size compared to the thermal gold film. The hardness and Young's modulus of the thermal and e-beam gold films were calculated to be 1.02–1.24 GPa & 90.53 102.02 GPa and 0.39–1.94 GPa & 76.31–155.20 GPa, respectively, at a load of 20–50 μN. The transmission line model (TLM) structure with pattern (Au/p-HgCdTe) was fabricated using the optimal gold films that were first established. In comparison to the thermally evaporated gold film (ρc =1.1 ×10 -2 Ωcm2), the e-beam evaporated TLM structure yielded a more Ohmic gold-contact with a small contact resistivity (ρc =7.3 ×10-3 Ωcm2). Therefore, to manufacture HgCdTe infrared detectors, e-beam-evaporated gold thin films might be utilized to provide an attractive and suitable Ohmic p-contact. Consequently, the enhanced characteristics of these thin films (CdTe, ZnS, CdS, Sn, In, and Cr Au) establish them as strong potential for incorporation into advanced electro-optic devices, HgCdTe-based infrared detectors, and next-generation photovoltaics. | en_US |
| dc.language.iso | en | en_US |
| dc.relation.ispartofseries | TD-9298; | - |
| dc.subject | FABRICATION | en_US |
| dc.subject | INSULATING THIN FILMS | en_US |
| dc.subject | SEMICONDUCTOR DEVICES | en_US |
| dc.subject | X-RAY DIFFRACTION ANALYSIS | en_US |
| dc.subject | ZINC SULFIDE (ZnS) | en_US |
| dc.title | FABRICATION AND CHARACTERIZATION OF METAL AND INSULATING THIN FILMS FOR SEMICONDUCTOR DEVICES | en_US |
| dc.type | Thesis | en_US |
| Appears in Collections: | Ph.D. Mechanical Engineering | |
Files in This Item:
| File | Description | Size | Format | |
|---|---|---|---|---|
| SHAILENDRA KUMAR GAUR Ph.D..pdf | 9.7 MB | Adobe PDF | View/Open | |
| SHAILENDRA KUMAR GAUR plag.pdf | 11.49 MB | Adobe PDF | View/Open |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.